banner
+

Anti-fingerprint Agent for Metal Resistance

Short Description
Fluorosilicone Polymer Anti-fingerprint Agent for Metal Materials.
1. Waterproof.
2. Oil resistance, anti-fingerprint. Stain Resistance.
3. Reduce friction coefficient.
4. Easy to clean.
5. High wear resistance.

<b><div>Short Description</div></b> Fluorosilicone Polymer Anti-fingerprint Agent for Metal Materials.</br> 1. Waterproof.</br> 2. Oil resistance, anti-fingerprint. Stain Resistance.<br> 3. Reduce friction coefficient.<br> 4. Easy to clean.<br> 5. High wear resistance. <br>

Short Description
Fluorosilicone Polymer Anti-fingerprint Agent for Metal Materials.
1. Waterproof.
2. Oil resistance, anti-fingerprint. Stain Resistance.
3. Reduce friction coefficient.
4. Easy to clean.
5. High wear resistance.

所属分类:

这里是占位文字

这里是占位文字

这里是占位文字

这里是占位文字

这里是占位文字

这里是占位文字

CONTACT US
  • PRODUCT DETAIL
  • APPLICATIONS SCOPE
  • PRODUCT TAGS
    • Commodity name: Anti-fingerprint Agent for Metal Resistance

    <b><div>Short Description</div></b> Fluorosilicone Polymer Anti-fingerprint Agent for Metal Materials.</br> 1. Waterproof.</br> 2. Oil resistance, anti-fingerprint. Stain Resistance.<br> 3. Reduce friction coefficient.<br> 4. Easy to clean.<br> 5. High wear resistance. <br>

    Product Paramenters

    Product Model DM200
    Appearance Transparent
    Solid Content 20%
    Application Metal materials field
    Function Anti-fingerprint, Oil resistance,Stain resistance
    Initial Water Contact Angle 110°-120°
    Storage In an airtight container (20°C).
    Storage Life 1 year (from the date of production)

     

    Introduction

    Fluorine-containing polymer surface treatment agent, by forming a monomolecular film sequential thin film coating on the surface of metal materials, it has excellent waterproof, oil resistance, antifouling and lubricating properties without affecting the appearance of the product. It can be coated by spraying, dipping, vacuum plating, etc.

     

    Application: Coating Technology

    1.Evaporation

    Suggested Coating Conditions:
    1. Substrate: After cleaning, it needs to be dried before use
    2. Equipment: vacuum coating machine
    3. Vacuum degree: less than 7.0E-3 Pa
    4. Film thickness of vacuum coating: SiO2, 8~10nm; AF, 10~17nm

    2.Spray Coating

    Suggested coating conditions:
    1. Equipment: spraying machine
    2. The main agent is used after being diluted according to the performance requirements
    3. Substrate: after cleaning, it needs to be dried before use
    4. The water droplet angle of the substrate after plasma treatment is less than 40°
    5. Liquid output: 30~70g/M2
    6. Baking conditions: 150-170℃, baking for 30 minutes

    3.Soaking

    Suggested coating conditions:
    1. Equipment: Container
    2. The main agent is used after being diluted according to the performance requirements
    3. Substrate: after cleaning, it needs to be dried before use
    4. The water droplet angle of the substrate after plasma treatment is less than 40°
    5. Soaking time: more than 1 minute
    6. Take-out speed: 5~15mm/sec
    6. Baking conditions: 150-170℃, baking for 30 minutes

  • Scope of Application

    Anti-fingerprint Agent for metal can be used at metal materials, like phone cover lens, back cover, escalator, Indoor elevator,kitchenware, metal tableware, etc.

     

     

  • Metal resistant agent

    AF agent

    hydrophobic agent

    nano coating hydrophobic

    Metal water repellent

    stainless steel sheet for wall panel oil and water repellent

PRODUCT DETAIL

Product Paramenters

Product Model DM200
Appearance Transparent
Solid Content 20%
Application Metal materials field
Function Anti-fingerprint, Oil resistance,Stain resistance
Initial Water Contact Angle 110°-120°
Storage In an airtight container (20°C).
Storage Life 1 year (from the date of production)

 

Introduction

Fluorine-containing polymer surface treatment agent, by forming a monomolecular film sequential thin film coating on the surface of metal materials, it has excellent waterproof, oil resistance, antifouling and lubricating properties without affecting the appearance of the product. It can be coated by spraying, dipping, vacuum plating, etc.

 

Application: Coating Technology

1.Evaporation

Suggested Coating Conditions:
1. Substrate: After cleaning, it needs to be dried before use
2. Equipment: vacuum coating machine
3. Vacuum degree: less than 7.0E-3 Pa
4. Film thickness of vacuum coating: SiO2, 8~10nm; AF, 10~17nm

2.Spray Coating

Suggested coating conditions:
1. Equipment: spraying machine
2. The main agent is used after being diluted according to the performance requirements
3. Substrate: after cleaning, it needs to be dried before use
4. The water droplet angle of the substrate after plasma treatment is less than 40°
5. Liquid output: 30~70g/M2
6. Baking conditions: 150-170℃, baking for 30 minutes

3.Soaking

Suggested coating conditions:
1. Equipment: Container
2. The main agent is used after being diluted according to the performance requirements
3. Substrate: after cleaning, it needs to be dried before use
4. The water droplet angle of the substrate after plasma treatment is less than 40°
5. Soaking time: more than 1 minute
6. Take-out speed: 5~15mm/sec
6. Baking conditions: 150-170℃, baking for 30 minutes