Antistatic Anti-fingerprint Agent
3. Reduce friction coefficient.
4. Easy to clean.
5. High wear resistance,Antistatic.
6. Improve acid and alkali resistance.
<b><div>Short Description</div></b> Fluorosilicone Polymer Anti-fingerprint Agent for Antistatic.</br> 1. Waterproof.</br> 2. Oil resistance,anti-fingerprint.<br> 3. Reduce friction coefficient.<br> 4. Easy to clean.<br> 5. High wear resistance,Antistatic. <br> 6. Improve acid and alkali resistance. <br>
3. Reduce friction coefficient.
4. Easy to clean.
5. High wear resistance,Antistatic.
6. Improve acid and alkali resistance.
所属分类:
这里是占位文字
这里是占位文字
这里是占位文字
这里是占位文字
这里是占位文字
这里是占位文字
- PRODUCT DETAIL
- APPLICATIONS SCOPE
- PRODUCT TAGS
-
- Commodity name: Antistatic Anti-fingerprint Agent
<b><div>Short Description</div></b> Fluorosilicone Polymer Anti-fingerprint Agent for Antistatic.</br> 1. Waterproof.</br> 2. Oil resistance,anti-fingerprint.<br> 3. Reduce friction coefficient.<br> 4. Easy to clean.<br> 5. High wear resistance,Antistatic. <br> 6. Improve acid and alkali resistance. <br>
Product Paramenters
Product Model Antistatic Anti-fingerprint Agent Appearance Transparent Solid Content 20% Application Antistatic for glass materials field Function Anti-fingerprint, oil-resistant,abrasive resistant, Antistatic Initial Water Contact Angle 110°-120° Storage In an airtight container (20°C). Storage Life 1 year (from the date of production) Introduction
Fluorine-containing polymer surface treatment agent, by forming a monomolecular film sequential thin film coating on the surface of glass, and it have a good adhesive resistance. it has excellent Antistatic, waterproof, oil resistance, antifouling and lubricating properties without affecting the appearance of the product. It can be coated by spraying, dipping, vacuum plating, etc.
Application: Coating Technology
1.Evaporation
Suggested Coating Conditions:
1. Substrate: After cleaning, it needs to be dried before use
2. Equipment: vacuum coating machine
3. Vacuum degree: less than 7.0E-3 Pa
4. Film thickness of vacuum coating: SiO2, 8~10nm; AF, 10~17nm2.Spray Coating
Suggested coating conditions:
1. Equipment: spraying machine
2. The main agent is used after being diluted according to the performance requirements
3. Substrate: after cleaning, it needs to be dried before use
4. The water droplet angle of the substrate after plasma treatment is less than 40°
5. Liquid output: 30~70g/M2
6. Baking conditions: 150-170℃, baking for 30 minutes3.Soaking
Suggested coating conditions:
1. Equipment: Container
2. The main agent is used after being diluted according to the performance requirements
3. Substrate: after cleaning, it needs to be dried before use
4. The water droplet angle of the substrate after plasma treatment is less than 40°
5. Soaking time: more than 1 minute
6. Take-out speed: 5~15mm/sec
6. Baking conditions: 150-170℃, baking for 30 minutes -
Scope of Application
Antistatic Anti-fingerprint Agent can be used at glass materials, like phone cover lens, back cover, phones display, glasses, camera lens, car touching panel, etc.
-
Antistatic agent
AF agent
hydrophobic agent
nano coating hydrophobic
glass water repellent for Antistatic
PRODUCT DETAIL
Product Paramenters
Product Model | Antistatic Anti-fingerprint Agent |
Appearance | Transparent |
Solid Content | 20% |
Application | Antistatic for glass materials field |
Function | Anti-fingerprint, oil-resistant,abrasive resistant, Antistatic |
Initial Water Contact Angle | 110°-120° |
Storage | In an airtight container (20°C). |
Storage Life | 1 year (from the date of production) |
Introduction
Fluorine-containing polymer surface treatment agent, by forming a monomolecular film sequential thin film coating on the surface of glass, and it have a good adhesive resistance. it has excellent Antistatic, waterproof, oil resistance, antifouling and lubricating properties without affecting the appearance of the product. It can be coated by spraying, dipping, vacuum plating, etc.
Application: Coating Technology
1.Evaporation
Suggested Coating Conditions:
1. Substrate: After cleaning, it needs to be dried before use
2. Equipment: vacuum coating machine
3. Vacuum degree: less than 7.0E-3 Pa
4. Film thickness of vacuum coating: SiO2, 8~10nm; AF, 10~17nm
2.Spray Coating
Suggested coating conditions:
1. Equipment: spraying machine
2. The main agent is used after being diluted according to the performance requirements
3. Substrate: after cleaning, it needs to be dried before use
4. The water droplet angle of the substrate after plasma treatment is less than 40°
5. Liquid output: 30~70g/M2
6. Baking conditions: 150-170℃, baking for 30 minutes
3.Soaking
Suggested coating conditions:
1. Equipment: Container
2. The main agent is used after being diluted according to the performance requirements
3. Substrate: after cleaning, it needs to be dried before use
4. The water droplet angle of the substrate after plasma treatment is less than 40°
5. Soaking time: more than 1 minute
6. Take-out speed: 5~15mm/sec
6. Baking conditions: 150-170℃, baking for 30 minutes